How much high temperature can polyurethane withstand?

Share This Post

How much high temperature can polyurethane withstand?

How much high temperature can polyurethane withstand
Polyurethane is a polymer material mainly polymerized from diisocyanates, chain extenders, and oligomer polyols, which has the comprehensive properties of rubber and plastic. It has excellent mechanical properties, wear resistance, oil resistance, tear resistance, chemical corrosion resistance, radiation resistance, and good adhesion. However, its usage temperature generally does not exceed 80 ℃. Materials above 100 ℃ will soften and deform, and its mechanical properties are significantly weakened. The short-term usage temperature does not exceed 120 ℃

Due to the good thermal stability of ester groups and the easy oxidation of hydrogen on the carbon atoms of ether groups, polyester based polyurethane has better heat resistance than polyether based polyurethane. The polyurethane prepared from polyester has little effect on its thermal properties due to the different types of polyester.

BOSS is a good partner of polyurethane PU seals.Tell us what you need.

Read More

Top 6 Seal Materials for Chemical Pumps and Valves

Six elastomers and plastics cover nearly every chemical pump duty. Ranked by where they earn their cost, with pH and temperature envelopes, four sealing positions inside one pump, and the traps a compatibility chart never shows.