PS017(Z5)

PS017 Z5 是一款用於雙作用氣壓缸的活塞密封件,採用 U 型杯設計並整合導向功能。另提供耐高溫版本

描述

PS017 Z5 氣動活塞密封

PS017 Z5 是一款用於雙作用氣動氣缸的活塞密封,採用 U 形杯設計並整合導向功能。另備有耐高溫版本。

Z5 氣動活塞密封工作環境

溫度:
NBR:0 ° C / +80 ° C
FKM:0 ° C/ +250 ° C
介質:油潤滑空氣以及乾燥空氣和無油空氣(裝配所需的初級潤滑)。
壓力:16 bar
速度:<1m/s
介質:壓縮空氣,含油及無油均可(安裝時需塗抹潤滑脂)

Z5 氣動密封尺寸:

氣動活塞密封 Z5 NBR N3578 FKM

 

 

零件編號.DdHd1L1L2L3右1右2
Z5 1610161010.513.51234.50.90.2
Z51812181210.515.51234.50.90.2
Z5 2014201410.517.51234.50.90.2
Z5 251825181222.513351.30.2
Z5 2822282210.525.51234.50.90.2
Z5 302330231227.513351.30.2
Z5 322532251229.513351.30.2
Z5 352835281232.513351.30.2
Z5 403340331237.513351.30.2
Z5 453845381242.513351.30.2
Z5 504350431247.513351.30.2
Z5 544654461351.51545.51.30.2
Z5 63536353176019571.60.3
Z5 635663561260.513351.30.3
Z5 700770621367.51545.51.60.3
Z5 76667666187320671.60.3
Z5 806780721377.41545.51.60.3
Z5 80708070187720671.60.3
Z5 A088100882196.52387.51.60.4
Z5 A08910090169718471.60.3
Z5 C5111251131512217561.60.4
Z5 C51312511321121.52387.51.60.4
Z5 D0171301201712719571.60.3
Z5 E02814012821136.52387.51.60.4
Z5 F0141501401714719571.60.3
Z5 G04516014526155.529109.51.60.4
Z5 L08520018526195.529109.51.60.4