Material:NBR/HNBR
Application:Auto,Constrution machinery

Описание

Rubber oil seal IUH

IUH rod seal as a smaller cross section shape, mainly used in a light duty applications,has good sealing effect work together with LBH wiper seal.

Технические данные
Давление: 20 МПа
Temperature: -20  to +100℃
Speed:  ≤1m/s
Material: NBR/HNBR

Color:Black

Dimensions:

ID*OD*H (mm)ID*OD*H (mm)ID*OD*H (mm)ID*OD*H (mm)
10*20*775*68*10135*150*9
19*27*675*88*10140*155*9
20*30*675*90*9145*160*10
22*32*680*90*6145*160*9
25*33*680*93*10150*165*10
25*35*780*95*10155*170*10
28*40*980*95*9160*175*10
30*40*785*100*10160*180*12
30*40*885*100*9165*180*10
35*43*685*105*12170*190*12
35*45*790*100*6170*195*15
35*45*890*105*10180*200*9
35*50*990*105*9180*205*15
40*50*690*110*12190*210*12
40*55*995*110*10195*215*12
45*55*895*110*9195*215*9
45*70*1295*115*12200*220*12
50*60*6100*115*9210*230*12
50*60*7100*120*12220*240*12
50*63*10105*120*10250*270*12
50*65*10105*120*9280*305*18
50*65*9105*125*12
50*70*10110*125*10
54*60*9110*125*9
55*65*6110*130*12
55*68*10115*130*10
55*70*9115*130*9
60*70*6115*135*12
60*73*10120*135*9
60*75*9120*140*10
62*78*10120*140*12
65*80*9125*140*9
70*83*10130*145*9
70*85*9130*150*12