Descrizione
Rubber oil seal IUH
IUH rod seal as a smaller cross section shape, mainly used in a light duty applications,has good sealing effect work together with LBH wiper seal.
Dati tecnici
Pressure: 20 MPa
Temperatura: da -20 a +100℃
Speed: ≤1m/s
Material: NBR/HNBR
Color:Black
Dimensioni:
| ID*OD*H (mm) | ID*OD*H (mm) | ID*OD*H (mm) | ID*OD*H (mm) |
| 10*20*7 | 75*68*10 | 135*150*9 | |
| 19*27*6 | 75*88*10 | 140*155*9 | |
| 20*30*6 | 75*90*9 | 145*160*10 | |
| 22*32*6 | 80*90*6 | 145*160*9 | |
| 25*33*6 | 80*93*10 | 150*165*10 | |
| 25*35*7 | 80*95*10 | 155*170*10 | |
| 28*40*9 | 80*95*9 | 160*175*10 | |
| 30*40*7 | 85*100*10 | 160*180*12 | |
| 30*40*8 | 85*100*9 | 165*180*10 | |
| 35*43*6 | 85*105*12 | 170*190*12 | |
| 35*45*7 | 90*100*6 | 170*195*15 | |
| 35*45*8 | 90*105*10 | 180*200*9 | |
| 35*50*9 | 90*105*9 | 180*205*15 | |
| 40*50*6 | 90*110*12 | 190*210*12 | |
| 40*55*9 | 95*110*10 | 195*215*12 | |
| 45*55*8 | 95*110*9 | 195*215*9 | |
| 45*70*12 | 95*115*12 | 200*220*12 | |
| 50*60*6 | 100*115*9 | 210*230*12 | |
| 50*60*7 | 100*120*12 | 220*240*12 | |
| 50*63*10 | 105*120*10 | 250*270*12 | |
| 50*65*10 | 105*120*9 | 280*305*18 | |
| 50*65*9 | 105*125*12 | ||
| 50*70*10 | 110*125*10 | ||
| 54*60*9 | 110*125*9 | ||
| 55*65*6 | 110*130*12 | ||
| 55*68*10 | 115*130*10 | ||
| 55*70*9 | 115*130*9 | ||
| 60*70*6 | 115*135*12 | ||
| 60*73*10 | 120*135*9 | ||
| 60*75*9 | 120*140*10 | ||
| 62*78*10 | 120*140*12 | ||
| 65*80*9 | 125*140*9 | ||
| 70*83*10 | 130*145*9 | ||
| 70*85*9 | 130*150*12 |