채팅 상담, 제공: LiveChat

신규 공급업체의 씰 품질 감사 방법(입고 검사 가이드)

신규 씰 공급업체를 위한 실용적인 입고 감사: AQL 샘플링, 광학 치수 검사, Shore A / 밀도 / 압축 영구 변형의 동일성 삼요소, ISO 3601-3 외관 등급 판정, 그리고 문제를 조기에 포착하는 서류 작업.

이 게시물 공유하기

A new supplier quotes 30% below your current source, the samples look clean, the certificates arrive as polished PDFs. Now comes the part that actually decides whether switching is safe: the incoming audit. Seal defects rarely show up as dramatic flaws — they hide in a hardness reading five points off spec, a cross-section 0.05 mm over tolerance, or a compression set number nobody asked for. This guide lays out the inspection sequence we recommend to importers and distributors when they onboard a new seal manufacturer, based on how our own quality team prepares shipments for third-party inspection.

Seal quality control bench with caliper, durometer and O-ring samples

Start With the Acceptance Criteria, Not the Parts

The most common audit failure happens before any measurement: nobody defined what “pass” means. An inspection without pre-agreed criteria turns every borderline result into a negotiation. Before the first carton is opened, write down four things:

  • The size standard. Which dimension system governs — AS568 dash numbers, ISO 3601 metric codes, or a customer drawing — and which tolerance class within it.
  • The material specification. Polymer family, hardness band (e.g., NBR 70 ±5 Shore A), and any mandatory certifications (FDA 21 CFR 177.2600, NSF/ANSI 61, WRAS, RoHS/REACH declarations).
  • The sampling plan. AQL levels per ANSI/ASQ Z1.4 (equivalently ISO 2859-1). Typical incoming practice for seals: AQL 1.0 for dimensional and visual defects, 2.5 for minor cosmetic items; critical applications go tighter.
  • The disposition rule. What happens on failure — re-inspection of double sample, lot rejection, or conditional release with a corrective action request. Decide this in advance or the audit becomes a debate.

One practical point on sampling: inspect by lot, not by carton. Mixed cartons from different production batches make every statistical conclusion meaningless. If the packing list shows two batch numbers, sample both separately.

Dimensional Check: Where Tolerances Are Won or Lost

Diameter and cross-section are the two numbers that decide whether a seal works at all. For O-rings, measure ID and cross-section (CS) against the tolerance band in ISO 3601-1 or the AS568 table. The method matters more than the instrument: soft rubber deforms under a caliper jaw, so calipers are a rough-screening tool only — fine for catching a grossly wrong part, not for conformance decisions.

Conformance-grade measurement uses a non-contact optical system (profile projector or vision measuring machine) that records the cord silhouette without touching it. If your inspection bench has no optics, measure CS with a micrometer against a mandrel-free method or use a cone gauge for ID, and note in the report that data is screening-level. We walk through the manual technique — including the cross-section measurement error most people make — in our guide to O링을 올바르게 측정하는 방법, which applies to the standard O-ring and X-ring stock most incoming lots contain.

For non-O-ring profiles (U-cups, V-packing, wipers), check the dimensions that interact with hardware: lip contact diameter, section height, and free state width. Record ambient temperature; a seal measured at 30°C is measurably larger than one measured at 18°C, and that difference is comparable to a tolerance band.

확인 항목InstrumentGoverning StandardTypical Incoming AQL
ID, CS, OD of O-ringsOptical comparator / vision systemISO 3601-1 / AS5681.0
Profile dimensions (lips, height)Profile projector, mandrel gaugesDrawing / manufacturer standard1.0
Hardness (Shore A)Durometer per ASTM D2240ISO 48-4 / ASTM D22401.0
Visual / surface defects10x magnifier, digital microscopeISO 3601-3 grades2.5
Weight / density (identity screen)0.001 g balanceCompound specPer lot

Material Identity: The Three-Test Triad

A black rubber part can be anything from EPDM to FKM — visually they are identical, and a wrong compound installed in the wrong fluid is a failure in weeks, not years. Three cheap tests identify most material substitutions without a laboratory:

경도. Shore A durometer per ASTM D2240 / ISO 48-4 is the first fingerprint. Take five readings on the part or on a spare sample, average them, and compare against spec. The standard molded tolerance is ±5 Shore A; a “70 Shore A NBR” averaging 78 is a different compound and must trigger a certificate check. Note the technique rules that keep readings honest: minimum sample thickness of 6 mm to avoid the anvil effect, readings at least 6 mm from any edge, and a 3-hour conditioning at 23 ± 2°C first. Thin O-rings measured directly on a standard durometer read artificially high — use a micro-IRHD instrument instead. The measurement technique rules — conditioning, dwell time, minimum thickness, edge distance — are laid out in detail in this Shore A testing guide, and a structured walkthrough of the whole six-stage incoming-to-final inspection framework is available from Detroit Sealing if you want a second opinion on sequencing.

Density. Weigh the part, weigh it suspended in water, and compute specific gravity. Every compound has a characteristic density band; a result outside it means wrong filler loading or a blend substitution. The test costs minutes and needs a 0.001 g balance.

압축 영구 변형. The strongest predictor of real-world sealing life. Per ISO 815 or ASTM D395 Method B, the sample is compressed 25%, held at temperature (22-72 h depending on the spec), and the unrecovered deformation is measured. Well-vulcanized compounds come back with set under about 20-25%; values in the 40s and beyond indicate under-cure, wrong recipe, or recycled stock. If you already maintain a reference library from an approved supplier, this is the test that exposes process differences between factories fastest. We explain what the numbers mean physically in our article on compression set.

When a dispute survives all three tests, escalate to FTIR spectroscopy (ASTM D3677 identifies the polymer family) and thermogravimetric analysis (ASTM D6370 quantifies filler and rubber content). Those require a lab, but they settle arguments — most independent labs quote per-sample and turn the result around within days.

Visual and Surface Inspection

Damaged polyurethane hydraulic seal laid out on an inspection bench

Visual inspection under 10x magnification is a screening step, never the verdict — but it catches the defect classes that dimensional checks miss entirely. Work through the parting line, the sealing surfaces, and the body in that order:

  • Flash and trim quality. Excess flash at the parting line, or trim that has torn a notch into the sealing surface, predicts leakage and assembly damage.
  • Porosity and pits. Gas entrapment during molding leaves voids that weep under pressure — most common on thick-section parts.
  • Blisters and internal voids. These are the explosive decompression risk markers: a blister that survives molding may rupture in high-pressure gas service.
  • Contamination and inclusions. Embedded foreign matter, mold release residue, discoloration — each is a batch-process signal.
  • Surface texture anomalies. Flow lines and dull patches can indicate cold molding; they matter on dynamic lips more than on static bodies.

ISO 3601-3 grades surface imperfections into class N (general purpose), S (higher surface quality) and CS (critical service). Ask the supplier which class their process targets, then inspect to that class — the grade defines how large an imperfection may be at a given size, so it converts visual opinion into a pass/fail. For machined parts, the surface and edge quality conversation is different; we covered the trade-offs in our molded versus machined seals comparison.

Laboratory Tests Worth Paying For

Not every incoming lot needs a lab. Reserve these for qualification of a new supplier, or for lots feeding critical applications:

  • Fluid immersion (ASTM D471 / ISO 1817). Soak samples in the actual working fluid at service temperature for 70 h, then measure volume change and hardness shift. Acceptance is typically within about ±10% volume change; large swell means the compound is not what the certificate claims.
  • Hot-air aging (ISO 188 / ASTM D573). 70 h at an elevated temperature, then compare tensile and hardness against the unaged values. This exposes under-cured compounds months before they harden in the field.
  • Tensile and elongation (ISO 37 / ASTM D412). The baseline mechanical screen; most hydraulic seal compounds target tensile strength above roughly 10-17 MPa with elongation above 200%, per the compound spec.

If the supplier offers a first-article report with these results, spot-verify one property yourself — hardness is the easiest — and treat agreement (or disagreement) as the real signal about the report’s credibility.

Paperwork and Traceability

Documents are part of the audit, and in regulated markets they are as binding as the dimensions. Collect and file: certificate of conformity tied to the actual batch number (a CoC without batch traceability is decoration), material data sheet with the compound code, certification copies relevant to your market (FDA, NSF, WRAS, RoHS/REACH declarations), and the production date or cure date. Serious manufacturers make their material documentation easy to audit — the sealing divisions of Trelleborg 와 Precision Polymer Engineering are good benchmarks for what a complete data package looks like. Then check shelf life against ISO 2230 storage rules — elastomers age in the warehouse, and a lot produced four years ago has consumed much of its usable life before you install it. Our article on rubber shelf life under ISO 2230 lists the standard storage windows by polymer.

Mark every sample you keep with lot and date, and keep retained samples from every accepted lot for at least one order cycle. When a field failure appears two batches later, the retained sample is the only way to prove whether the problem arrived with the goods or developed in service.

Red Flags That Should Stop a Shipment

ObservationProbable Root CauseRecommended Disposition
Hardness average off by more than 5 points, or uneven across partsWrong compound or uncontrolled cureHold lot; request batch certs; reject if unexplained
Compression set above ~30% in the spec testUnder-cure or filler substitutionReject; require compound corrective action
Blisters or porosity on sealing surfacesMolding process faultReject; 100% screen or full lot return
Density outside the compound bandFiller loading or blend substitutionHold; escalate to FTIR/TGA verification
CoC lacks batch numbers or cure datesTraceability system gapConditional release only; audit required before next lot
Mixed batches packed in one cartonPacking QC breakdownSample each batch separately; note for supplier scorecard

One caution as you build the program: a single failed check rarely condemns a supplier — a single hidden one does. Suppliers who volunteer bad data (an honest compression set at 28%, a batch they quarantined themselves) are usually safer partners than those whose paperwork is flawless but arrives only when asked. Weight the audit toward what a supplier measures when nobody is watching, and the incoming inspection becomes what it should be: a fast confirmation, not a rescue mission.

실행 체크리스트

  • Write the acceptance criteria first: size standard, hardness band, certifications, AQL per ANSI/ASQ Z1.4, and the failure disposition rule.
  • Sample by production batch, never by carton; keep retained samples from every accepted lot.
  • Measure dimensions optically where possible; treat caliper readings as screening only.
  • Run the identity triad on every qualification: Shore A (ISO 48-4), density, and compression set (ISO 815 / ASTM D395 Method B).
  • Inspect visually to an ISO 3601-3 surface class under 10x magnification — flash, porosity, blisters, inclusions.
  • Reserve fluid immersion and aging tests for new-supplier qualification and critical applications.
  • Verify CoC batch traceability, cure dates, and shelf life against ISO 2230 before the lot enters your warehouse.

If the audit load exceeds your bench capacity, independent inspection agencies and full-line distributors such as ERIKS offer incoming QC services — worth considering for high-volume lots until your own routine is established.

더 보기

셰브론 씰(V-패킹)이란? 적층형 V-링 세트 설명

수 어댑터, 적층형 자기 가압 V-링, 암 어댑터: 링 개수가 압력 등급을 결정하는 방식, 마모된 실린더가 셰브론 세트를 용서하는 이유, 그리고 글랜드 조정이 현장에서 누출 없는 운전 시간을 확보하는 방법.