“Seventy durometer, black” is the most common line on an O-ring inquiry we receive, and it is roughly as complete a specification as “blue, medium-sized car.” Hardness is one number out of a material callout that needs at least six, and the number itself carries a tolerance wide enough to hide a real difference in behavior. Still, it is the fastest measurement a buyer can make on a receiving dock, and it is the first thing a seal engineer asks for when a leak comes back.

This guide covers what the instrument measures, which scale applies to which material, why a 70 ± 5 callout is normal and what it costs you, and where hardness stops being informative — including the substitutions it will never catch.

Seal quality control bench with digital caliper, durometer and O-ring samples

What the Instrument Actually Measures

A durometer presses a defined indenter into the material under a defined spring force and reads how far it penetrates, converted to a 0–100 scale where higher means harder. The geometry of the indenter, the spring rate and the foot diameter are all fixed by standard, which is why a reading from one calibrated instrument can be compared with another — and why an uncalibrated one cannot.

Two standards cover the same measurement in different regions. ASTM D2240 governs the Shore scales used across North America; ISO 7619-1 covers rubber in Europe and Asia, and ISO 868 covers plastics. The scales are numerically compatible for practical purposes, but the test conditions differ in small ways, so a certificate quoting ISO 7619-1 and an incoming check run to ASTM D2240 will not agree to the point.

For thin or curved parts, neither flat-foot method works well. An O-ring of 2.62 mm cross-section cannot present the flat, thick surface the standard assumes, and the presser foot bridges the curve. That is where IRHD micro-hardness testing to ISO 48 comes in: a small ball indenter under low load, designed for exactly these geometries. Labs that test O-rings properly use it, and the readings sit within a few points of a Shore A value taken on a molded button of the same compound.

Three Scales, One Question

The scales are not interchangeable, and using the wrong one produces numbers that look plausible and mean nothing.

ScaleIndenterRange it coversTypical seal-shop use
ショアATruncated cone, bluntSoft to medium elastomers, roughly 20–95Every rubber seal, gasket and sheet product; the default for O-rings
Shore DSharp 30° coneHard rubber and rigid plastics, roughly 40–90PTFE, PEEK, nylon and other machined sealing parts
IRHD micro (ISO 48)Small ball, low loadThin and curved sectionsFinished O-rings and small molded seals where a flat specimen is impossible

The overlap zone confuses people. There is no exact conversion between Shore A and Shore D because the indenter geometries differ; published tables exist, and they are approximations that hold only in the 90 A to 55 D band. A part specified at 95 Shore A and a part specified at 45 Shore D are not the same thing even though a conversion chart suggests they are close.

For the materials our customers machine rather than mold, the Shore D values are the ones that matter: unfilled PTFE sits around 50–65 Shore D, and PEEK around 85–90 Shore D. That spread explains a design behavior we see in the field — PTFE back-up rings conform and seal well but cold-flow under load, PEEK back-up rings hold their geometry and carry load but conform less. Material suppliers such as Victrex publish the full mechanical picture, and our machined engineering plastics range is specified in Shore D for this reason.

Why 70 ± 5 Is a Band, Not a Number

Almost every rubber seal datasheet reads 70 ± 5 Shore A, and the tolerance is not a supplier’s excuse — it reflects real process scatter. Compound mixing, cure gradients across a mold, post-cure and part geometry all move the reading by a few points, and the standard tolerance band absorbs that. A “70 durometer” seal is therefore anything from about 65 to 75, and both ends are conforming product.

Measurement adds its own scatter on top. The standard requires a specimen thick enough that the indenter does not feel the surface underneath — 6 mm is the usual minimum — a flat surface, full contact of the presser foot, and a defined dwell time before the reading is taken. Best practice is five readings at least 6 mm apart, with the median reported. Test a 3 mm cord on a steel bench and the indenter reads the bench; test a warm part straight out of a wash station and it reads soft; press and read instantly on a viscoelastic compound and the number drifts while you watch it.

Two practical consequences. First, do not reject a lot on a single reading — reject on a median of five taken correctly, ideally on a molded button from the same batch. Second, put the test method and specimen type in your specification. “70 ± 5 Shore A per ASTM D2240 on a 6 mm button” is enforceable; “70 durometer” invites an argument your inspector cannot win.

Hardness band (Shore A)Behavior適合する用途
40–50Very conformable, low seating stress, poor extrusion resistanceLight flange gaskets, rough or warped sealing faces, low pressure only
60–70Balanced; the industrial defaultGeneral O-rings, pneumatic seals, oil seals, water and air service
80Firmer, better extrusion resistance, needs more squeeze forceHydraulic static seals, higher pressures, larger clearance gaps
90Hard, minimal conformabilityHigh-pressure hydraulic dynamic seals, usually with a back-up ring
95+Near-rigid elastomer; behaves more like a plasticSpecialty high-pressure seats and wear parts

How Hardness Changes What the Seal Does

Hardness is a proxy for modulus, and modulus decides two competing behaviors that every seal design balances.

Conformability. A softer compound flows into surface imperfections and seals against a rougher face at lower load. That is why 50–60 Shore A appears on low bolt-load flanges and on covers that are clamped by hand. The cost is extrusion: under pressure, soft rubber flows into the clearance gap, gets nibbled off at the gap edge, and the seal fails from the outside in. Our article on extrusion at high pressure walks through the gap arithmetic.

Extrusion resistance. A harder compound resists being pushed into the gap, which is why high-pressure hydraulic seals move to 80–90 Shore A. The cost is the opposite one: a hard ring needs more squeeze force to seal at low pressure, so it can weep on a system that idles at 2 bar and seals perfectly at 200 bar.

O-ring compressed in a steel gland groove cross-section showing squeeze

Friction and breakaway. Harder compounds generally produce higher breakout force in dynamic service, and in pneumatic cylinders that shows up as stick-slip rather than as a leak. If low friction is the design driver, hardness is a secondary lever next to profile and surface finish — covered in our guide to low-friction pneumatic seals.

圧縮永久ひずみ。 Hardness and compression set interact in a way that catches buyers who shop on hardness alone. Two compounds can both read 70 Shore A and diverge by a factor of three in compression set at 100 °C, because set is driven by cure system and base polymer, not by modulus. A seal that hardens in service and one that takes a permanent set both lose sealing force, and the durometer reading after service will not distinguish them. The mechanism is covered in our article on 圧縮永久ひずみ.

Hardness by Seal Type and Duty

Selection tables are starting points, not answers, but the industry defaults are stable enough to be useful.

用途代表的な硬度理由
Pneumatic cylinder seals70 Shore A, 60 for very low pressureLow load, need conformability at low differential pressure; friction matters
Hydraulic static O-rings70–80 Shore ABalance of squeeze and extrusion resistance in a confined groove
Hydraulic dynamic rod and piston seals80–90 Shore A (PU often 90–95 Shore A)Pressure and gap; polyurethane grades sit harder than rubber at equal duty
Rotary shaft oil seals70–80 Shore A lip compoundLip must follow shaft runout without excessive radial load
Flange and cover gaskets50–70 Shore ABolt load is limited; conformability dominates
Back-up rings (PTFE / PEEK)50–65 Shore D / 85–90 Shore DStructural role; measured on the plastic scales, not Shore A

Note the polyurethane line. PU rod seals commonly specify 90–95 Shore A, harder than the equivalent NBR seal, because the material’s higher tensile strength and tear resistance allow a harder, more extrusion-resistant part without the brittleness a rubber compound would show at that hardness. Comparing a 93 Shore A PU seal with a 70 Shore A NBR seal as if hardness were the variable is comparing two different design intents.

What a Durometer Reading Cannot Tell You

Hardness is cheap to check and therefore over-trusted. Four things it will not reveal:

Which polymer you received. NBR, EPDM and FKM can all be compounded to 70 Shore A. A durometer cannot distinguish them, and neither can a visual check. Density is the fastest field screen: FKM compounds run around 1.80–1.90 g/cm³, NBR around 1.20–1.30, EPDM around 1.10–1.25. A 70 Shore A ring that should be FKM and weighs like NBR is NBR. Confirmation comes from FTIR or DSC, but the balance catches most substitutions before the lab does.

Whether the compound suits the media. Two 70 Shore A rings can differ by 40 points of volume swell in the same oil. Immersion testing to ASTM D471, or a datasheet with real swell data, is the only evidence that matters.

Whether the part will hold its force. Compression set, stress relaxation and aging behavior all sit outside the hardness number.

Whether the surface will seal. A ring at nominal hardness with a parting-line ridge across the sealing face leaks, and the durometer reads perfectly. That is a visual acceptance question, governed by a grade like those in ISO 3601-3, not a hardness question.

Digital caliper measuring an O-ring cross-section on a workbench

Specifying Hardness Correctly

A complete hardness callout has four parts, and all four fit on one line of a purchase order.

1. The value and tolerance — “70 ± 5” rather than “70.” Anything tighter than ± 5 asks the molder for process capability the material does not naturally provide.

2. The scale — Shore A for elastomers, Shore D for plastics. Never a bare number.

3. The method and specimen — “per ASTM D2240 on a 6 mm molded button” or “IRHD micro per ISO 48 on the finished part.” This tells the supplier how the number will be measured and removes the argument at receiving.

4. The compound — polymer, grade and any certification, since hardness alone does not identify the material. Our O-ring and X-ring catalog lists hardness alongside compound and size code for exactly this reason, and The Engineering ToolBox is a reasonable reference for unit conversions when a drawing mixes scales, while distributor references such as Marco Rubber および Delta Rubber publish practical hardness guidance for stock ranges.

主なポイント

Hardness measures indentation resistance, not quality. It tells you how a compound behaves under load, not whether it suits your fluid, temperature or duty cycle.

70 ± 5 Shore A is the industrial default, and the band is real. Inspect on a median of five correct readings, not on one, and put the test method in the specification.

Shore A and Shore D are not convertible. Elastomer seals live on A; PTFE and PEEK parts live on D, and published conversion tables only hold in a narrow overlap.

Roughly 60–70 Shore A buys conformability, 80–90 buys extrusion resistance. Choose by pressure and gap first, then adjust for friction and low-pressure sealing.

A durometer cannot identify a polymer. Check density as a fast screen, then confirm with FTIR or DSC when a substitution would be expensive.

続きを読む

ショア硬度とは?シール購入者のための実践ガイド