V ring A dimensions:

SizeΦD1dD(d+2*c)cabΦD2ΦD3Assembly width B1
VA-32.7-3.52.55.51.52.13d1+1d1+62.5±0.3
VA-43.5-4.53.27.222.43.7d1+1d1+63±0.4
VA-54.5-5.54822.43.7d1+1d1+63±0.4
VA-65.5-6.55922.43.7d1+1d1+63±0.4
VA-76.5-861022.43.7d1+1d1+63±0.4
VA-88-9.571122.43.7d1+1d1+63±0.4
VA-109.5-11.591533.45.5d1+1d1+94±0.6
VA-1211.5-13.510.516.533.45.5d1+1d1+94±0.6
VA-1312.5-13.511.716.533.45.5d1+1d1+94±0.6
VA-1413.5-15.512.518.533.45.5d1+1d1+94±0.6
VA-1615.5-17.5142033.45.5d1+1d1+94±0.6
VA-1817.5-19162233.45.5d1+1d1+94±0.6
VA-2019-21182644.77.5d1+2d1+126±0.8
VA-2221-24202844.77.5d1+2d1+126±0.8
VA-2524-27223044.77.5d1+2d1+126±0.8
VA-2827-29253344.77.5d1+2d1+126±0.8
VA-3029-31273544.77.5d1+2d1+126±0.8
VA-3231-33293744.77.5d1+2d1+126±0.8
VA-3533-36313944.77.5d1+2d1+126±0.8
VA-3836-38344244.77.5d1+2d1+126±0.8
VA-4038-43364655.59d1+2d1+157±1
VA-4543-48405055.59d1+2d1+157±1
VA-5048-53455555.59d1+2d1+157±1
VA-5553-58495955.59d1+2d1+157±1
VA-6058-63546455.59d1+2d1+157±1
VA-6563-68586855.59d1+2d1+157±1
VA-7068-73637566.811d1+3d1+189±1.2
VA-7573-78677966.811d1+3d1+189±1.2
VA-8078-83728466.811d1+3d1+189±1.2
VA-8583-88768866.811d1+3d1+189±1.2
VA-9088-93819366.811d1+3d1+189±1.2
VA-9593-98859766.811d1+3d1+189±1.2
VA-10098-1059010266.811d1+3d1+189±1.1
VA-110105-1159911377.912.8d1+4d1+2110.5±1.5
VA-120115-12510812277.912.8d1+4d1+2110.5±1.5
VA-130125-13511713177.912.8d1+4d1+2110.5±1.5
VA-140135-14512614077.912.8d1+4d1+2110.5±1.5
VA-150145-15513514977.912.8d1+4d1+2110.5±1.5
VA-160155-1651441608914.5d1+4d1+2412±1.8
VA-170165-1751531698914.5d1+4d1+2412±1.8
VA-180175-1851621788914.5d1+4d1+2412±1.8
VA-190185-1951711878914.5d1+4d1+2412±1.8
VA-199195-2101801988914.5d1+4d1+2412±1.8
VA-200190-2101802101514.325d1+10d1+4520±4
VA-220210-2351982281514.325d1+10d1+4520±4
VA-250235-2652252551514.325d1+10d1+4520±4
VA-275265-29024701514.325d1+10d1+4520±4
VA-300290-3102703001514.325d1+10d1+4520±4
VA-325310-3352923221514.325d1+10d1+4520±4
VA-350335-3653153451514.325d1+10d1+4520±4
VA-375365-3903373671514.325d1+10d1+4520±4
VA-400390-4303603901514.325d1+10d1+4520±4
VA-450430-4804054351514.325d1+10d1+4520±4
VA-500480-5304504801514.325d1+10d1+4520±4
VA-550530-5804955251514.325d1+10d1+4520±4
VA-600580-6305405701514.325d1+10d1+4520±4
VA-650630-6656006301514.325d1+10d1+4520±4
VA-700665-7056306601514.325d1+10d1+4520±4
VA-725705-7456707001514.325d1+10d1+4520±4
VA-750745-7857057351514.325d1+10d1+4520±4
VA-800785-8307457751514.325d1+10d1+4520±4
VA-850830-8707858151514.325d1+10d1+4520±4
VA-900875-9208258551514.325d1+10d1+4520±4
VA-950920-9658658951514.325d1+10d1+4520±4
VA-1000965-10159109401514.325d1+10d1+4520±4
VA-10501015-10659559851514.325d1+10d1+4520±4
VA-10601015-106595598598514.325d1+10d1+4520±4
VA-11001065-111510001030103014.325d1+10d1+4520±4
VA-11501115-116510451075107514.325d1+10d1+4520±4
VA-12001165-121510901120112014.325d1+10d1+4520±4
VA-12501215-127011351165116514.325d1+10d1+4520±4
VA-13001270-132011801210121014.325d1+10d1+4520±4
VA-13501320-137012251255125514.325d1+10d1+4520±4
VA-14001370-142012701300130014.325d1+10d1+4520±4

 

For further information,please request

For other rubber seals requirement,please click: Guarnizioni in gomma

Tags: V-ring seals

Richiedi un preventivo

Contattaci oggi stesso e ricevi una revisione aziendale e una consulenza gratuite.