Petearje mei ús, mooglik makke troch LiveChat

V-RING TYPE A

V RING SEAL VA,VDA

Beskriuwing

V-ring type A is in gewoane net-druk elastyske rubberen ôfdichtingsring foar rotearjende as. De ôfdichtingslippe hat goede beweeglikheid en oanpassingsfermogen. It kin grutte tolerânsjes en hoekôfwikingen kompensearje en it ynkringen fan ekstern wetter en stof foarkomme.

De VA-type ôfdichting kin brûkt wurde foar it ôfdichtsjen en reparearjen en reparearjen fan it haadprodukt. It is gewoan yn 'e anty-kâld ôfdichting fan waskapparatuer en rôljende staven.

V ring A diminsjes:

GrutteΦD1dD(d+2*c)cabΦD2ΦD3Montearring breedte B1
VA-32.7-3.52.55.51.52.13d1+1d1+62.5±0.3
VA-43.5-4.53.27.222.43.7d1+1d1+63±0.4
VA-54.5-5.54822.43.7d1+1d1+63±0.4
VA-65.5-6.55922.43.7d1+1d1+63±0.4
VA-76.5-861022.43.7d1+1d1+63±0.4
VA-88-9.571122.43.7d1+1d1+63±0.4
VA-109.5-11.591533.45.5d1+1d1+94±0.6
VA-1211.5-13.510.516.533.45.5d1+1d1+94±0.6
VA-1312.5-13.511.716.533.45.5d1+1d1+94±0.6
VA-1413.5-15.512.518.533.45.5d1+1d1+94±0.6
VA-1615.5-17.5142033.45.5d1+1d1+94±0.6
VA-1817.5-19162233.45.5d1+1d1+94±0.6
VA-2019-21182644.77.5d1+2d1+126±0.8
VA-2221-24202844.77.5d1+2d1+126±0.8
VA-2524-27223044.77.5d1+2d1+126±0.8
VA-2827-29253344.77.5d1+2d1+126±0.8
VA-3029-31273544.77.5d1+2d1+126±0.8
VA-3231-33293744.77.5d1+2d1+126±0.8
VA-3533-36313944.77.5d1+2d1+126±0.8
VA-3836-38344244.77.5d1+2d1+126±0.8
VA-4038-43364655.59d1+2d1+157±1
VA-4543-48405055.59d1+2d1+157±1
VA-5048-53455555.59d1+2d1+157±1
VA-5553-58495955.59d1+2d1+157±1
VA-6058-63546455.59d1+2d1+157±1
VA-6563-68586855.59d1+2d1+157±1
VA-7068-73637566.811d1+3d1+189±1.2
VA-7573-78677966.811d1+3d1+189±1.2
VA-8078-83728466.811d1+3d1+189±1.2
VA-8583-88768866.811d1+3d1+189±1.2
VA-9088-93819366.811d1+3d1+189±1.2
VA-9593-98859766.811d1+3d1+189±1.2
VA-10098-1059010266.811d1+3d1+189±1.1
VA-110105-1159911377.912.8d1+4d1+2110.5±1.5
VA-120115-12510812277.912.8d1+4d1+2110.5±1.5
VA-130125-13511713177.912.8d1+4d1+2110.5±1.5
VA-140135-14512614077.912.8d1+4d1+2110.5±1.5
VA-150145-15513514977.912.8d1+4d1+2110.5±1.5
VA-160155-1651441608914.5d1+4d1+2412±1.8
VA-170165-1751531698914.5d1+4d1+2412±1.8
VA-180175-1851621788914.5d1+4d1+2412±1.8
VA-190185-1951711878914.5d1+4d1+2412±1.8
VA-199195-2101801988914.5d1+4d1+2412±1.8
VA-200190-2101802101514.325d1+10d1+4520±4
VA-220210-2351982281514.325d1+10d1+4520±4
VA-250235-2652252551514.325d1+10d1+4520±4
VA-275265-29024701514.325d1+10d1+4520±4
VA-300290-3102703001514.325d1+10d1+4520±4
VA-325310-3352923221514.325d1+10d1+4520±4
VA-350335-3653153451514.325d1+10d1+4520±4
VA-375365-3903373671514.325d1+10d1+4520±4
VA-400390-4303603901514.325d1+10d1+4520±4
VA-450430-4804054351514.325d1+10d1+4520±4
VA-500480-5304504801514.325d1+10d1+4520±4
VA-550530-5804955251514.325d1+10d1+4520±4
VA-600580-6305405701514.325d1+10d1+4520±4
VA-650630-6656006301514.325d1+10d1+4520±4
VA-700665-7056306601514.325d1+10d1+4520±4
VA-725705-7456707001514.325d1+10d1+4520±4
VA-750745-7857057351514.325d1+10d1+4520±4
VA-800785-8307457751514.325d1+10d1+4520±4
VA-850830-8707858151514.325d1+10d1+4520±4
VA-900875-9208258551514.325d1+10d1+4520±4
VA-950920-9658658951514.325d1+10d1+4520±4
VA-1000965-10159109401514.325d1+10d1+4520±4
VA-10501015-10659559851514.325d1+10d1+4520±4
VA-10601015-106595598598514.325d1+10d1+4520±4
VA-11001065-111510001030103014.325d1+10d1+4520±4
VA-11501115-116510451075107514.325d1+10d1+4520±4
VA-12001165-121510901120112014.325d1+10d1+4520±4
VA-12501215-127011351165116514.325d1+10d1+4520±4
VA-13001270-132011801210121014.325d1+10d1+4520±4
VA-13501320-137012251255125514.325d1+10d1+4520±4
VA-14001370-142012701300130014.325d1+10d1+4520±4

 

Foar mear ynformaasje, freegje it oan

Foar oare easken foar rubberen ôfdichtingen, klikje hjir: Rubberôfdichtingen

Labels: V-ring ôfdichtingen

Freegje in offerte oan

Nim hjoed kontakt mei ús op en krije in fergees bedriuwsresinsje en konsultaasje.