تحدث معنا, ، مدعوم بواسطة LiveChat

الوصف

V-ring type A is a common non-pressure elastic rubber sealing ring for rotating shaft. The sealing lip has good mobility and adaptability. It can compensate for large tolerances and angular deviations and prevent the intrusion of external water and dust.

The VA type seal can be used for sealing and repairing and repairing the main product. It is common in the anti-cold seal of washing equipment and rolling bars.

V ring A dimensions:

SizeΦD1dD(d+2*c)cabΦD2ΦD3Assembly width B1
VA-32.7-3.52.55.51.52.13d1+1d1+62.5±0.3
VA-43.5-4.53.27.222.43.7d1+1d1+63±0.4
VA-54.5-5.54822.43.7d1+1d1+63±0.4
VA-65.5-6.55922.43.7d1+1d1+63±0.4
VA-76.5-861022.43.7d1+1d1+63±0.4
VA-88-9.571122.43.7d1+1d1+63±0.4
VA-109.5-11.591533.45.5d1+1d1+94±0.6
VA-1211.5-13.510.516.533.45.5d1+1d1+94±0.6
VA-1312.5-13.511.716.533.45.5d1+1d1+94±0.6
VA-1413.5-15.512.518.533.45.5d1+1d1+94±0.6
VA-1615.5-17.5142033.45.5d1+1d1+94±0.6
VA-1817.5-19162233.45.5d1+1d1+94±0.6
VA-2019-21182644.77.5d1+2d1+126±0.8
VA-2221-24202844.77.5d1+2d1+126±0.8
VA-2524-27223044.77.5d1+2d1+126±0.8
VA-2827-29253344.77.5d1+2d1+126±0.8
VA-3029-31273544.77.5d1+2d1+126±0.8
VA-3231-33293744.77.5d1+2d1+126±0.8
VA-3533-36313944.77.5d1+2d1+126±0.8
VA-3836-38344244.77.5d1+2d1+126±0.8
VA-4038-43364655.59d1+2d1+157±1
VA-4543-48405055.59d1+2d1+157±1
VA-5048-53455555.59d1+2d1+157±1
VA-5553-58495955.59d1+2d1+157±1
VA-6058-63546455.59d1+2d1+157±1
VA-6563-68586855.59d1+2d1+157±1
VA-7068-73637566.811d1+3d1+189±1.2
VA-7573-78677966.811d1+3d1+189±1.2
VA-8078-83728466.811d1+3d1+189±1.2
VA-8583-88768866.811d1+3d1+189±1.2
VA-9088-93819366.811d1+3d1+189±1.2
VA-9593-98859766.811d1+3d1+189±1.2
VA-10098-1059010266.811d1+3d1+189±1.1
VA-110105-1159911377.912.8d1+4d1+2110.5±1.5
VA-120115-12510812277.912.8d1+4d1+2110.5±1.5
VA-130125-13511713177.912.8d1+4d1+2110.5±1.5
VA-140135-14512614077.912.8d1+4d1+2110.5±1.5
VA-150145-15513514977.912.8d1+4d1+2110.5±1.5
VA-160155-1651441608914.5d1+4d1+2412±1.8
VA-170165-1751531698914.5d1+4d1+2412±1.8
VA-180175-1851621788914.5d1+4d1+2412±1.8
VA-190185-1951711878914.5d1+4d1+2412±1.8
VA-199195-2101801988914.5d1+4d1+2412±1.8
VA-200190-2101802101514.325d1+10d1+4520±4
VA-220210-2351982281514.325d1+10d1+4520±4
VA-250235-2652252551514.325d1+10d1+4520±4
VA-275265-29024701514.325d1+10d1+4520±4
VA-300290-3102703001514.325d1+10d1+4520±4
VA-325310-3352923221514.325d1+10d1+4520±4
VA-350335-3653153451514.325d1+10d1+4520±4
VA-375365-3903373671514.325d1+10d1+4520±4
VA-400390-4303603901514.325d1+10d1+4520±4
VA-450430-4804054351514.325d1+10d1+4520±4
VA-500480-5304504801514.325d1+10d1+4520±4
VA-550530-5804955251514.325d1+10d1+4520±4
VA-600580-6305405701514.325d1+10d1+4520±4
VA-650630-6656006301514.325d1+10d1+4520±4
VA-700665-7056306601514.325d1+10d1+4520±4
VA-725705-7456707001514.325d1+10d1+4520±4
VA-750745-7857057351514.325d1+10d1+4520±4
VA-800785-8307457751514.325d1+10d1+4520±4
VA-850830-8707858151514.325d1+10d1+4520±4
VA-900875-9208258551514.325d1+10d1+4520±4
VA-950920-9658658951514.325d1+10d1+4520±4
VA-1000965-10159109401514.325d1+10d1+4520±4
VA-10501015-10659559851514.325d1+10d1+4520±4
VA-10601015-106595598598514.325d1+10d1+4520±4
VA-11001065-111510001030103014.325d1+10d1+4520±4
VA-11501115-116510451075107514.325d1+10d1+4520±4
VA-12001165-121510901120112014.325d1+10d1+4520±4
VA-12501215-127011351165116514.325d1+10d1+4520±4
VA-13001270-132011801210121014.325d1+10d1+4520±4
VA-13501320-137012251255125514.325d1+10d1+4520±4
VA-14001370-142012701300130014.325d1+10d1+4520±4

 