Beskriuwing

Tapassings en eigenskippen
This product with the anti-wear and piston ring used in combination to prevent the cylinder oil mixed
with foreign matters and cause damage to the seals and to ensure that the seals have a long service life.The piston rod seals,used in combine with oil pressure,prevent to store up of oil pressure.
Standertmaterialen
bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE
Wurkbetingsten
Diameter Range: from 50 mm to 200 mm
Temp Range: -200℃ to +200℃
Speed: <=1.5 m/s
Medium: Algemien petroleum-basearre hydraulyske oalje, wetter/glykol hydraulyske oalje, oalje/wetter emulsje,hydraulyske oalje.