WSZ

Product description: PTFE Wiper Seal WSZ

Beskriuwing

1. Tapassingen en eigenskippen

For reciprocating system,especially in low temperature,high frequency and heavy dust conditions.

mainly applied to hydraulic and pneumatic devices,servo system,chemical and food machinery.Excellent sliding performance,no stick-slip behavior,no viscosity,compensates to the distortion of pistons and plungers,excellent compatibility of hydraulic mediums,excellent effect of scraping residue oil films of the rod surface from inside.

2. Standertmaterialen

Glidring: brûnsfol PTFE, koalstofvezelfol PTFE, grafytfol PTFE

O-ring: NBR/FKM. oar materiaal is beskikber.

3. Wurkbetingsten

Diameter Range: from 20mm to 1000mm

Drukberik: 0-60 MPa

Tempberik: -30℃ oant 200℃

Snelheid: <=5m/s

Medium: hydraulyske oalje, wetter, lucht, amper ûntflambere fluids.

Other general seal profile name:DSZ,GSZ