Beskriuwing
The AED O-ring adopts a special formulation process to greatly improve the high-strength performance of the rubber, so that it has strong tear resistance during the rapid pressure relief process under high pressure conditions, and has excellent resistance to petroleum gas and medium performance.
Product Series:
FKM AED O-ring, FKM GLT AED low temperature explosion-proof O-ring, HNBR AED O-ring
Temperature range:
FKM AED type: – 30 ° C ~ 220 ° C
FPM AED type: – 45°C ~ 220°C
FKM GFLT AED type: -40°C~230°C
HNBR AED type: – 45 ° C ~ 180 ° C