JUNTA TOROIDAL AED

FKM/FPM AED resist
HNBR resist
High pressure withstand
Customized AED rubber seal
Product description: FKM AED resist o-ring and rubber seals HNBR AED withstand o ring and seals

Descrição

The AED O-ring adopts a special formulation process to greatly improve the high-strength performance of the rubber, so that it has strong tear resistance during the rapid pressure relief process under high pressure conditions, and has excellent resistance to petroleum gas and medium performance.

Product Series:
FKM AED O-ring, FKM GLT AED low temperature explosion-proof O-ring, HNBR AED O-ring

Temperature range:
FKM AED type: – 30 ° C ~ 220 ° C
FPM AED type: – 45°C ~ 220°C
FKM GFLT AED type: -40°C~230°C
HNBR AED type: – 45 ° C ~ 180 ° C