Chat with us, powered by LiveChat

Top 8 Engineering Plastics for Sealing-Related Wear Parts

Eight plastics cover almost every wear part next to a seal. PV limits, temperature ceilings and the constraint that should pick the material for you.

Share This Post

The seal gets the attention; the wear part next to it decides whether the assembly survives. Guide rings, wear bands, backup rings, bushings, valve seats and scraper pads all fail by wear before the elastomer lip beside them does — and the material you pick for those parts is a plastics decision, not a seal decision. Eight engineering plastics cover almost every wear part in industrial equipment. This guide compares them with real PV limits, temperature ceilings and cost factors, then maps each material to the parts it wins.

PEEK sealing rings and machined engineering plastic wear parts arranged on a workshop bench

The Number That Rules Wear Parts: PV

For any dry-running bearing or wear surface, the controlling parameter is the PV limit: bearing pressure (P) times sliding velocity (V) beyond which frictional heat outruns the material’s ability to shed it, and wear stops being gradual. Below the limit, the part wears slowly and predictably. Above it, thermal softening takes over and the part fails in hours.

Three practical rules follow from that definition:

  • Design to half the limit. Continuous operation should stay near 50% of the published PV limit; intermittent duty can touch 75% if the part gets time to cool between cycles.
  • Temperature derates everything. A nylon bushing rated near 5,000 psi-fpm at 20°C may hold only 1,500–2,000 psi-fpm at 80°C as stiffness drops.
  • Manufacturer data beats family data. Family-level figures (the ones below) are screening numbers; a filled grade from one supplier can outrun the family average by a wide margin.

The Eight Materials, Side by Side

The figures below are drawn from the Quadrant Engineering Plastic Products design and fabrication guide, one of the most widely referenced bearing-grade comparison tables in the industry. Values are for dry sliding against steel; lubricated service multiplies the limits.

Table 1: Bearing-grade plastics — wear-relevant properties (dry vs steel)
MaterialContinuous tempLimiting PV (psi·fpm)Wear factor kDynamic frictionCost factor
UHMWPE82°C (180°F)2,000110.120.5
Acetal (POM-C/POM-H)82°C (180°F)2,7002000.251.2
Nylon PA6/PA66 (unfilled)93°C (200°F)2,700–3,00075–1000.20–0.251.0
Nylon + oil/solid lube (NSM type)93°C (200°F)15,000–17,00012–260.14–0.181.4–1.5
Filled PTFE (Fluorosint type)260°C (500°F)8,000–20,00030–6000.10–0.1512
PPS (Techtron type)221°C (430°F)8,750–25,00062–8000.2018–22
PEEK (unfilled / filled / HPV)249°C (480°F)8,500–25,000100–3750.20–0.4020–55
PAI (Torlon/Duratron type)260°C (500°F)22,50010–450.2028

Two things jump out of that table. First, the internally lubricated nylon (the oil-filled NSM class) is the biggest PV bargain on the list — five to six times the limiting PV of unfilled nylon at barely half the price of PEEK. Second, cost is not monotonic with performance: UHMWPE at half the cost of nylon wins outright in wet, abrasive, slow service where PEEK would be expensive overkill.

For a closer treatment of how filler systems change the base polymer, our earlier guide on PEEK sealing components covers the carbon- and glass-filled PEEK grades in sealing service specifically.

Match the Material to the Binding Constraint

Material selection for wear parts is easier if you ask which constraint binds first: load, speed, temperature, friction, or environment. Each column of the table has a clear winner.

Table 2: Which plastic wins which constraint
Binding constraintFirst choiceWhy it wins
Highest dry load + speed (high PV)PAI, then filled PEEKPV 22,500 psi·fpm at 260°C continuous
High temperature + chemical exposurePPS, then PEEK221–249°C service with broad chemical resistance
Lowest friction, dry runningFilled PTFEμ 0.10–0.15 with fillers fixing PTFE’s cold-flow problem
Wet, dirty, abrasive, slowUHMWPEBest abrasion resistance, near-zero water absorption, cheapest
Precision + low cost, moderate dutyAcetalDimensionally stable, machines cleanly, low water uptake
Cheapest acceptable dry PVInternally lubricated nylon15,000+ psi·fpm at cost factor 1.4
Extreme temperature (300°C+)Polyimide (PI)316°C continuous, PV to 37,500–40,000 in PI/PBI grades

Machined engineering plastic rods and finished wear components from a stock-shape supplier

Mapping Materials to Sealing-Adjacent Parts

The eight materials map onto the common wear parts around seals with surprising little overlap. The assignments below reflect what actually fails in field service and what suppliers stock as standard shapes.

Table 3: Part-by-part material recommendations
Wear partDefault materialUpgrade pathRationale
Hydraulic guide rings / wear bandsPTFE + bronze, or phenolic fabricPEEK for high side loadsLow friction against chrome; PEEK when load spikes crush softer bands
Pneumatic cylinder bearingsAcetal or filled nylonUHMWPE where moisture is presentDry-running, low stick-slip, low cost at high volume
Backup rings (anti-extrusion)PTFE, nylon, UHMWPEPEEK above ~40 MPa or high tempStiffness to bridge the extrusion gap without scoring the gland
Valve seats and balls-guidesFilled PTFEPAI or PEEK for high pressure differentialSealing conformance plus wear resistance
Rotary shaft bearings (dry)Lube-filled nylonPEEK HPV / PAI above 100°CInternal lubricant carries the PV load without grease
Scraper / wiper wear pads (conveyors, buckets)UHMWPENylon where heat buildsAbrasion king at the lowest cost per part
Pump wear rings (chemical service)PPS or PEEKCarbon-filled PEEK for dry-start toleranceChemical resistance plus dimensional stability at temperature

Note how rarely unfilled PEEK is the right answer despite its reputation. Filled and internally lubricated grades (the HPV/CA30 class) carry roughly three times the PV of virgin PEEK because the fillers interrupt the wear mechanism instead of letting adhesive wear run against a smooth polymer surface. The same logic applies to our guide ring and wear band selection guide, where the fill system decides the band’s load rating.

Machining, Moisture and the Details That Change the Answer

Three second-order effects regularly overturn a table-based selection:

Moisture swelling. Nylon absorbs 1.5–2.5% water in 24-hour immersion and keeps going over weeks; running clearances specified for dry nylon seize in wet service. Acetal and UHMWPE absorb almost nothing. If the part sees water, emulsion or washdown, nylon either gets a moisture-compensated clearance or loses the job.

Cold flow (creep). Unfilled PTFE creeps under sustained load — it is why neat PTFE bushings collapse and why filled grades exist. Any PTFE part under sustained compression needs filler content or a design that limits preload.

Surface finish of the counterface. Plastic bearings want a steel counterface around 0.2–0.4 μm Ra. Much rougher and the plastic abrades itself; much smoother and adhesive wear takes over because no micro-reservoirs of transfer film form. This mirrors the shaft-finish discipline for hydraulic seals — the counterface matters as much as the polymer.

Manufacturing route matters too, particularly for volumes. Standard stock shapes (rod, tube, sheet) machined on CNC cover prototypes and low-to-mid volumes economically; molded production parts win above thousands of pieces. The trade-offs are laid out in our molded vs machined comparison, and the same economics apply to wear parts as to seals.

Running Clearances and Thermal Growth

Plastic bushings run hotter and expand more than the steel around them. Typical thermal expansion coefficients run five to ten times that of steel — roughly 50–80 × 10⁻⁶/°C for most of these polymers versus about 12 for steel — so a clearance that works at ambient can close up at operating temperature. Standard practice for plastic plain bearings sets running clearance at 0.3–0.8% of shaft diameter to absorb thermal growth and moisture swelling together; tighter than that risks seizure, looser than that costs precision and edge loading.

Bushing proportions matter as much as clearance. A length-to-diameter ratio between roughly 0.8:1 and 1.5:1 keeps edge loading and frictional heat manageable: shorter than 0.8:1 and the bushing misaligns, longer than 1.5:1 and the ends carry disproportionate load as the shaft deflects. Wall thickness of 1.5–3 mm on small bores balances strength against heat transfer — plastic sheds frictional heat through the housing, so a chunky bushing insulates its own wear surface.

One more installation detail: plastics press-fit differently than bronze. Interference fits relax over time as the polymer creeps, so housings that rely on press-fit alone to locate a plastic bushing should pin or otherwise mechanically retain it. Every one of these rules trades against the PV table above — the material only delivers its rated wear life inside a geometry that keeps it cool and aligned.

Verifying Quality Before the First Production Run

Plastic wear parts are easy to specify and easy to get wrong in the supply chain. Virgin resin grades are straightforward; filled grades are where substitutions happen, because the filler system is invisible once the part is machined. Three checks that catch most problems:

  • Material certification. Ask for a certificate of conformity naming the exact grade (not just “PEEK” — the difference between virgin 450G and a carbon-filled CA30 grade is three times the PV limit), plus filler percentage where applicable.
  • Burn or density spot checks. Filled PTFE grades differ measurably in density with filler content; a quick density check against the datasheet flags a filled-vs-virgin substitution without a lab.
  • First-article dimensional audit at temperature. For precision parts, measure a machined part after thermal cycling to the expected service temperature. Hidden residual stress from aggressive machining shows up as drift that only appears in service.

Suppliers differ more on wear parts than on seals because the material market has more entry-level players. When evaluating a new source, benchmark against the stock-shape majors’ published data — and treat any quoted PV figure materially above the family values in Table 1 with healthy suspicion until it comes with test conditions attached. For the semi-finished stock shapes most of these parts start from, see our engineering plastics product range.

FAQ

Is PEEK always worth the premium over nylon or acetal?
No. PEEK earns its cost factor of 20–55 in high temperature, high PV or aggressive chemical service. A pneumatic bushing at 40°C and moderate load is a place where acetal or filled nylon does the same job for a tenth of the price. Buy PEEK where a constraint table says you must, not as insurance by default.

Can UHMWPE replace nylon everywhere it is cheaper?
Not quite. UHMWPE’s 82°C ceiling and its low stiffness exclude it from precision loaded parts and anything near hot oil. It wins on abrasion, wet environments and friction; it loses on stiffness, temperature and dimensional precision.

How do I verify a PV rating before committing a design?
Run the bearing pressure from your actual load and projected area, multiply by surface velocity, and keep continuous operation at or below half the published limit — then re-check at the maximum operating temperature, since PV limits derate sharply as material stiffness drops. For a worked method, the PV comparison reference at mechcodex walks through the screening calculation step by step.

Which material for a wear part that also has to seal?
Filled PTFE when chemical exposure or low friction dominates, PEEK when pressure differential or wear life dominates. The sealing function changes the question from pure wear to wear-plus-compression behavior, which favors the filled fluoropolymers and the stiffer high-performance polymers over commodity nylon.

Read More