Description
B-Wave Gasket – Multi-Lip Wave Seal for Static Joints
The B-Waveflon Gasket is an annular elastomer seal with several wave-shaped sealing lips. Under assembly compression the crests generate a sustained restoring force and form multiple continuous barriers between mating faces. Compared with a flat gasket it better accommodates minor flange irregularity, thermal movement and light vibration, making it an economical choice for bolted flange joints.
Key Features
- Multi-lip sealing: four wave lips contact the mating faces in sequence for staged compression and several leakage barriers.
- Elastic compensation: the wave profile provides controlled axial elasticity to absorb surface deviation, thermal cycling and light vibration.
- Lower stress concentration: load is distributed along the crests, avoiding local over-compression and helping long-term sealing.
- Flexible sizes and materials: standard DN15 to DN125, with FKM / EPDM / MVQ / CR and custom compounds matched to the medium.
Structure & Principle
The waveflon gasket uses a thin annular section with an axial width of about 4 mm. Four wave lips are arranged along the radial direction, with a lip pitch of about 2 mm and an edge radius of R1.5. De (outside diameter) and Di (inside diameter) determine the fit with the port or step; A / B / C / D are the reference diameters of the four wave lips from inside to outside. During compression the crests make contact progressively, forming a multi-stage seal from inside to outside.


Standard Dimensions (mm)
| DN | De (mm) | Di (mm) | A (mm) | B (mm) | c (mm) | D (mm) |
| DN15 | 51 | 22 | 25 | 32.6 | 40.3 | 48 |
| DN 20 | 61 | 27 | 30 | 39.3 | 48.7 | 58 |
| DN 25 | 71 | 34 | 37 | 47.3 | 57.7 | 68 |
| DN 32 | 82 | 43 | 46 | 57 | 68 | 79 |
| DN 40 | 92 | 49 | 52 | 64.3 | 76.7 | 89 |
| DN 50 | 107 | 61 | 64 | 77.3 | 90.7 | 104 |
| DN 65 | 127 | 77 | 80 | 94.6 | 109.3 | 124 |
| DN 80 | 1 42 | 89 | 92 | 107.6 | 123.3 | 139 |
| DN 100 | 162 | 115 | 118 | 131.6 | 145.3 | 159 |
| DN 125 | 192 | 1 41 | 1 44 | 159 | 1 74 | 189 |
| For selection reference only. Purchase drawings must be confirmed by both parties. | ||||||
Material Selection
| Material | Typical temp. | Key advantages | Suitable media | Main limitations |
| FKM | -20 to +200 °C | Heat, oil and chemical resistance | Mineral oil, fuels, aromatics, many acids | Not for hot water/steam or ketone/ester solvents |
| EPDM | -50 to +150°C | Water, steam, ozone and ageing resistance | Water, steam, coolants, brake fluids | Not resistant to mineral oils and greases |
| MVQ | -60 to +200。C | Wide range, non-toxic, insulating | Air, food contact, medical and electrical | L ower mechanical strength and oil resistance |
| CR | -30 to +110°C | Balanced oil/weather, flame retardant | Air, water, weak acids/alkalis, refrigerants | Not for aromatics or strong oxidisers |
| others | By grade | Custom solutions | Special chemicals, extreme temperatures | Technical review required |
Typical Applications
- Flanged pipe connections in water, oil and gas systems
- Chemical process lines and vessels
- Pumps, valves and skid-mounted equipment
- Water treatment facilities and static joints under vibration

Selection & Installation
Provide DN or De/Di with groove and step details, the medium and concentration, normal and peak temperature, pressure, vibration and static or dynamic use. Clean mating faces and remove burrs before assembly; cross-tighten evenly to avoid one-sided load. Avoid touching the sealing lips with sharp tools and avoid excessive compression.
Custom & Ordering
Non-standard dimensions, special materials and certification requirements can be developed from a drawing or sample. For a quick quotation please send size, material, medium, temperature, pressure, quantity, lead time and any certification or packing requirements.
Contact: Henry | Tel: +86 13392768056 | Email: sales@bosssealing.com
WhatsApp: +8613392768056 | Web: https://www.bosssealing.com
All illustrations are redrawn schematics for selection and technical communication only. Final selection must be validated under actual service conditions.
Tag:Wave Gasket, waveflon gasket,Gasket waveline