FEP (Fluorinated ethylene propylene) Introduction
FEP (Fluorinated ethylene propylene) Introduction FEP-fluorinated ethylene propylene copolymer FEP is tetrafluoroethylene and hexafluoropropylene copolymerization, also known as F46. FEP has a melting point of