Applications and properties
Be widely used in agricultural machinery,injection moulding machines,forklifts,cranes.
One no-standard seal and two o-ring energizer,scraper seal DPT1 improves the sealing effect,low
coefficient offriction,no stick-slip behavior.Excellent performance in locating and positioning.High
reliability,can accept full loadingworking pressure in a short time.
Standard material
Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE
O-Ring:NBR/FKM. other material is available.
Working conditions
Pressure Range:0-60 MPa
Temp Range: -30℃ to 200℃
Speed: <=5m/s
Medium:Hydraulic Oil,water,air barely flammable fluids.
Diameter Range:
from 20mm to 1000mm
Other seal profile name: PT1,DPT,JPT1,DPE