설명
적용 분야 및 특성
For reciprocating system,especially in low temperature,high frequency and heavy dust conditions.
mainly applied to hydraulic and pneumatic devices,servo system,chemical and food
machinery.Excellent sliding performance,no stick-slip behavior,no viscosity,compensatesto the
distortion of pistons and plungers,excellent compatibility of hydraulic mediums,excellent effect of
scraping residue oil films of the rod surface from inside.
표준 재질
슬라이드 링: 청동 충전 PTFE, 탄소 섬유 충전 PTFE, 흑연 충전 PTFE
O-링: NBR/FKM. 다른 재질도 사용 가능합니다.
3. 작동 조건
Diameter Range: from 5mm to 1000mm
압력 범위: 0-60 MPa
온도 범위: -30℃ ~ 200℃
속도: <=5m/s
매체: 유압유, 물, 공기, 난연성 유체.
other general seal profile name: WSZ2,DSZ2,DSZL