채팅 상담, 제공: LiveChat

AF

Product description: AF wiper seal,Hydraulic wipers AF,AF scraper seal

카테고리

설명

AF is a wiper with a metal framework which used in hydraulic applications to obstruct all kinds of negative foreign particles to go into the cylinders.
Standardized with the materials of high performance PU 93 shore A and Metal case.

Technical Data
Temperature: -35 to +100 ℃
Speed:  1m/s
Media: Hydraulic oils (mineral oil-based)

Material
Material: PU  Framework: Metal
Hardness: 93 ±2 Shore A
Color: Blue / Green / Light yellow

Advantages
High abrasion resistance.
Widely applicable.
Easy installation.

 