설명
DSDKI oil wiper seal
DSDKI DKI oil wiper seal, consist of a wiper lip and a metal frame, mainly used for open grooves, made of polyurethane material and metal material.
- Material: Lip Material: PU (NBR also available)
- 금속 프레임 재질: 금속
- 적용 주요 유체: 외부 먼지.
DKI oil wiper seal is widely used in hydraulic cylinders, construction machinery, press machines, agricultural machinery, elevators, industrial equipment, injection molding machines, etc.
기술 데이터:
온도: -20℃ ~ +100℃
Speed:≤ 1 m/s
매체: 유압 오일(광유 기반)
Material: PU 95 shore A
Color: Off-Yellow
DSDKI wiper seal size chart:
| 품목 | Dimension mm | 부품 번호. |
| DSDKI | 20x28x5/7 | DSDKI202857 |
| DSDKI | 20x30x7/10 | DSDKI2030710 |
| DSDKI | 22x32x7/10 | DSDKI2232710 |
| DSDKI | 25x35x7/10 | DSDKI2535710 |
| DSDKI | 30x40x5/7 | DSDKI304057 |
| DSDKI | 32x42x5/7 | DSDKI324257 |
| DSDKI | 32x42x7/10 | DSDKI3242710 |
| DSDKI | 32x45x7/10 | DSDKI3245710 |
| DSDKI | 36x46x7/10 | DSDKI3646710 |
| DSDKI | 36x45x7/10 | DSDKI3645710 |
| DSDKI | 36x48x5/8 | DSDKI364858 |
| DSDKI | 45x55x7/10 | DSDKI4555710 |
| DSDKI | 45x58x7/10 | DSDKI4558710 |
| DSDKI | 55x65x7/10 | DSDKI5565710 |
| DSDKI | 60x70x7/10 | DSDKI6070710 |
| DSDKI | 63x75x7/10 | DSDKI6375710 |
| DSDKI | 65x75x7/10 | DSDKI6575710 |
| DSDKI | 70x80x7/10 | DSDKI7080710 |
| DSDKI | 75x83x7/10 | DSDKI7583710 |
| DSDKI | 75x85x7/10 | DSDKI7585710 |
| DSDKI | 80x90x7/10 | DSDKI8090710 |
| DSDKI | 85x95x7/10 | DSDKI8595710 |
| DSDKI | 90x100x7/10 | DSDKI90100710 |
| DSDKI | 90x102x7/10 | DSDKI90102710 |
| DSDKI | 100x110x7/10 | DSDKI100110710 |
| DSDKI | 105x115x7/10 | DSDKI105115710 |
| DSDKI | 145x160x9/12 | DSDKI145160912 |
For non-standard sizes, please request.