oil seal
hydraulic compact piston seal
Material:NBR+PA
Application:Constrution machinery

説明

OUY OIL SEAL

OUY is mainly used for piston seals of tensioning cylinders of construction machinery such as forklifts, excavators, etc.Has the characteristics of wear resistance, high pressure resistance, aging resistance, corrosion resistance.

技術データ:    
Pressure:  ≤30 MPa
Temperature: -20℃ to +100℃
速度:0.5m/s
Material: NBR+PA

Sizes:

OD*ID*H (mm)
40*25*12
50*35*12
60*45*12
60*35*15.5
65*50*12
70*54*12
70*55*12
70*40*12
70*45*15.5
70*90*12
75*65*8
75*60*12
80*64*12
80*50*12
80*47*16
90*70*15
90*80*8
85*70*12
90*65*18
100*75*18
105*90*12
110*90*12
105*85*12
100*80*12
130*110*12
150*130*12
120*100*12