1. Applications and properties
Standard double acting seal.
For reciprocated hydraulic system,allow large extrusion gap,has wide application,high static and dynamic sealing effect,be able to work in dusty condition,low friction,available in various of materials.
2.Standard materials
Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE
Elastomer:NBR
Back up ring:Nylon/POM
3.Working conditions
Diameter Range: from 50mm to 1000mm
Pressure Range:0-50 MPa
Temp Range: -30℃ to 100℃
Speed: <=1.5m/s
Medium:Hydraulic Oil,water,air barely flammable fluids.
4.SPGW/PHD dimensions
please request.