Descrizione
OUY OIL SEAL
OUY is mainly used for piston seals of tensioning cylinders of construction machinery such as forklifts, excavators, etc.Has the characteristics of wear resistance, high pressure resistance, aging resistance, corrosion resistance.
Dati tecnici:
Pressure: ≤30 MPa
Temperature: -20℃ to +100℃
Velocità: 0,5 m/s
Material: NBR+PA
Sizes:
| OD*ID*H (mm) | |
| 40*25*12 | |
| 50*35*12 | |
| 60*45*12 | |
| 60*35*15.5 | |
| 65*50*12 | |
| 70*54*12 | |
| 70*55*12 | |
| 70*40*12 | |
| 70*45*15.5 | |
| 70*90*12 | |
| 75*65*8 | |
| 75*60*12 | |
| 80*64*12 | |
| 80*50*12 | |
| 80*47*16 | |
| 90*70*15 | |
| 90*80*8 | |
| 85*70*12 | |
| 90*65*18 | |
| 100*75*18 | |
| 105*90*12 | |
| 110*90*12 | |
| 105*85*12 | |
| 100*80*12 | |
| 130*110*12 | |
| 150*130*12 | |
| 120*100*12 |