Petearje mei ús, mooglik makke troch LiveChat

OUY

oalje sealing
hydraulic compact piston seal
Material:NBR+PA
Application:Constrution machinery

Beskriuwing

OUY OIL SEAL

OUY is mainly used for piston seals of tensioning cylinders of construction machinery such as forklifts, excavators, etc.Has the characteristics of wear resistance, high pressure resistance, aging resistance, corrosion resistance.

Technical Data:    
Pressure:  ≤30 MPa
Temperature: -20℃ to +100℃
Speed: 0.5m/s
Material: NBR+PA

Sizes:

OD*ID*H (mm)
40*25*12
50*35*12
60*45*12
60*35*15.5
65*50*12
70*54*12
70*55*12
70*40*12
70*45*15.5
70*90*12
75*65*8
75*60*12
80*64*12
80*50*12
80*47*16
90*70*15
90*80*8
85*70*12
90*65*18
100*75*18
105*90*12
110*90*12
105*85*12
100*80*12
130*110*12
150*130*12
120*100*12

Freegje in offerte oan