الوصف
وصلة فكية JC
JC is suitable for water pump and other mechanical equipment,has good pysical properties and easy-stallation properties.
Working conditions:
المادة: PU
Color:natural PU
Hardness:90-95 shore A
Torque:22.5-2500NM
المقاس: يُرجى الطلب
Relevant tags:pump shaft coupling,jaw coupling factory,buy jaw coupling,hydraulic shaft coupling,flexible spider coupling