الوصف
Coupling MT
MT is commonly used as shaft coupling elastor spiders in big mechanical equipments.
Working conditions:
Material:PU
Color:Red,Green,Blue,Yellow
Hardness:90-95 shore A
Torque:22.5-2500NM
Size:please request
Relevant tags:coupling MT,elastic coupling,gear coupling manufacturers,flexible rubber coupling,spider coupling