Описание
EU rod and wiper pneumatic seal has good function of sealing,dustproof and fixing.As the specially designed lips,it shows good properties of low-friction and long-service life.
Material&Temperature Range:
PU:0℃ ~ 100 ℃; FKM:-20℃ ~ 220 ℃;
Hardness:70 shore A
Pressure:≤1.6 MPa
Speed:≤1m/s

| Part no.: | d | D | H | D1 | L1 | L2 | R | f |
| EU12*19*10 | 12 | 19 | 10 | 21 | 7.7 | 12 | 1 | 1.5 |
| EU12*20*10.7 | 12 | 20 | 10.7 | 22 | 8.8 | 12 | 1.1 | 1.5 |
| EU12*22*10.7* | 12 | 22 | 10.7 | 24 | 8.8 | 12 | 1.1 | 1.5 |
| EU14*24*10.7 | 14 | 24 | 10.7 | 26 | 8.8 | 13 | 1.1 | 1.5 |
| EU16*26*10.7 | 16 | 26 | 10.7 | 28 | 8.8 | 13 | 1.1 | 1.5 |
| EU18*26*10.7* | 18 | 26 | 10.7 | 28 | 8.8 | 13 | 1.1 | 1.5 |
| EU18*28*10.7 | 18 | 28 | 10.7 | 30 | 8.8 | 13 | 1.1 | 1.5 |
| EU20*30*10.7 | 20 | 30 | 10.7 | 32 | 8.8 | 13 | 1.4 | 1.5 |
| EU22*32*11.2 | 22 | 32 | 11.2 | 34.5 | 9.4 | 14 | 1.4 | 2 |
| EU25*35*11.2 | 25 | 35 | 11.2 | 37.5 | 9.4 | 14 | 1.4 | 2 |
| EU30*40*11.2* | 30 | 40 | 11.2 | 42.5 | 9.4 | 14 | 1.4 | 1.5 |
| EU32*42*10.7* | 32 | 42 | 10.7 | 44.5 | 8.8 | 13 | 1.4 | 1.5 |
| EU32*42*11.2 | 32 | 42 | 11.2 | 44.5 | 9.4 | 14 | 1.4 | 2 |
| EU40*50*11.2 | 40 | 50 | 11.2 | 53.2 | 9.4 | 14 | 1.4 | 2 |
| EU45*55*12.2* | 45 | 55 | 12.2 | 58.2 | 10.4 | 15 | 1.8 | 2 |
| EU50*60*12.2 | 50 | 60 | 12.2 | 63.2 | 10.4 | 15 | 1.8 | 2 |
| EU63*75*13 | 63 | 75 | 13 | 78.2 | 11.4 | 16 | 1.8 | 2 |