Чат с нами, при поддержке LiveChat

Air compressor seal ring

G453/G418
PTFE+CARBON+GRAPHITE
Black
Oil free,luburicant
Product description: G453,G418,oil free,air compressor piston ring,black compressor seal

Описание

Air compressor piston seal ring

Esprecially designed for air compressor, has oil free,sel-lubricant, very good wear resistance and high temperature resistance properties.
Material:

G453,PTFE+23% carbon fiber+2% graphite

G418,PTFE+15% glass fiber + 5% Mos2

Customized air compressor seal rings are available and welcomed.