Air compressor piston seal ring
Esprecially designed for air compressor, has oil free,sel-lubricant, very good wear resistance and high temperature resistance properties.
Материал:
G453,PTFE+23% carbon fiber+2% graphite
G418,PTFE+15% glass fiber + 5% Mos2
Customized air compressor seal rings are available and welcomed.
Please contact:sales@bosssealing.com