MBN BRN3

U-seal back up ring
Nylon material
Mould pressing
Gray color
Product description: Nylon back-up ring for U seals

Descrição

Nylon back-up ring for U seal MBN, BRN3

Dados técnicos:
Material: Nylon
Temperature: -30℃ to 100℃
Pressure: 0-30MPa
Speed: 1m/s

Nylon backup ring MBN BRN3 size

ItemSize mm
MBN/BRN335*50*3
MBN/BRN340*50*3
MBN/BRN340*55*3
MBN/BRN345*55*3
MBN/BRN350*60*3
MBN/BRN350*63*3
MBN/BRN355*65*3
MBN/BRN355*68*3
MBN/BRN355*70*3
MBN/BRN360*70*3
MBN/BRN360*73*3
MBN/BRN360*80*3
MBN/BRN364*80*3
MBN/BRN365*75*3
MBN/BRN365*80*3
MBN/BRN365*80*3
MBN/BRN365*85*3
MBN/BRN370*80*3
MBN/BRN370*83*3
MBN/BRN370*85*3
MBN/BRN375*85*3
MBN/BRN375*88*3
MBN/BRN375*90*3
MBN/BRN375*95*3
MBN/BRN380*90*3
MBN/BRN380*93*3
MBN/BRN380*95*3
MBN/BRN380*100*3
MBN/BRN385*100*3
MBN/BRN385*105*3
MBN/BRN390*105*3
MBN/BRN390*110*3
MBN/BRN395*110*3
MBN/BRN395*115*3
MBN/BRN3100*115*3
MBN/BRN3100*120*3
MBN/BRN3105*120*3
MBN/BRN3105*125*3
MBN/BRN3110*125*3
MBN/BRN3110*130*3
MBN/BRN3115*130*3
MBN/BRN3115*135*3
MBN/BRN3120*135*3
MBN/BRN3120*140*3
MBN/BRN3130*145*3
MBN/BRN3130*150*3
MBN/BRN3140*160*3