Technical Data:
Pressure: 400 bar
Temperature: -35 to +100℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: PU
Hardness: 90-95 Shore A
Color: Blue/Green/Original
Advantages:
Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation