Descrição

1. Applications and properties
Be used in broad pressure and high slide speed working conditions,standard compact seals.
Low friction,good wear-resistance.
2.Standard materials
Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE
O-Ring:NBR/FKM. other material is available.
3.Working conditions
Diameter Range: from 18mm to 1000mm
Pressure Range:0-60 MPa
Temp Range: -30℃ to 200℃
Speed: <=1.5m/s
Medium:Hydraulic Oil,water,air barely flammable fluids.