Fale connosco, com tecnologia de LiveChat

PSD

Product description: Piston Seal PSD

Descrição

1. Applications and properties

Piston seal GSD is a standard double acting seal.

For reciprocated hydraulic system,allow large extrusion gap,has wide application,high static and             dynamic sealing effect,be able to work in dusty condition,low friction,available in various of

materials.

2.Standard materials

Slide Ring:bronze filled PTFE,carbon fiber filled PTFE,graphite filled PTFE

O-Ring:NBR/FKM. other material is available.

3.Size

Bore dia from 8mm to 1600mm