Fale connosco, com tecnologia de LiveChat

KYD

Product description: PISTON SEAL,PISTON U CUP, KYD

Descrição

Application: The sealing of piston rod in hydraulic cylinder under reciprocating movements.

Technical Data:
Pressure: 400 Bar
Temperature: NBR -35 to +110℃
Speed:  0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: PU
Hardness: 90-95 Shore A
Color: Blue/Green/Original

Advantages:

Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation