HBY

Rod buffer seal
buffer seal HBY
Product description: buffer seal,buffer seal HBY,HBY

Descrição

HBY is a buffer ring, due to a special structure, facing the sealing lip of the medium reduce the remaining seal formed between the pressure transmission back to the system.

Technical Data:
Pressure: below 50 MPa
Temperature: -35  to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: U cups:PU;Back-up ring:POM/PA
Hardness: 90-95 Shore A

Color:Blue,Purple,Off-Yellow

Size: Standard and non-standard

Pedir orçamento