Descrição
BAS consists of a PU lip seal and a high elastic NBR O-ring. The NBR O-ring in this design provides maximum sealing even in low pressures.
Technical Data
Pressure: 35 MPa
Temperature: -35 to +80 ℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material
Material: PU / O-ring: NBR
Hardness: 90 Shore A
Color: Blue
Advantages
Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation