Technical Data
Pressure:  40 MPa
Temperature: -35  to +100 ℃
Speed:  0.5m/s
Media: Hydraulic oils (mineral oil-based)

Material
Material: PU
Hardness: 90 Shore A
Color: Blue / Green / Original