채팅 상담, 제공: LiveChat

TB Oil Seal

Double lip
Iron Framework
High pressure resist
Product description: Double lip TB rotary shaft oil seal

카테고리

설명

TB oil seal

TB is a double lip oil seal, which can prevent lubricant leakage and prevent external foreign matter. It is suitable for rotary acting movements. Has good properties of easy-install and high pressure resitance.

Technical data:

Material: nitrile rubber NBR + iron shell; fluoro rubber FKM + iron shell;
Pressure: 0.3kgf/cm2
Temperature: NBR: -20 ° C / + 100 ° C; FKM: -20 ° C / + 200 ° C
Speed: NBR≤15 m/s; FKM≤25 m/s
Size: Please request.

견적 받기