VPC Vee packing Set

Vee packing
Seal Set
homogenizer packing
plunger packing seals
Product description: v packing seals sets,vee packing,packing seals for bow thruster

카테고리

설명

 

 

 

V packing seals, also called vee cups, v packings, vee packing sets, vee packing seal, etc. They are composed of 3-10 lip rings made of cotton fiber reinforced rubber elastomer.

Boss Sealing Solutions vee packing seals are suitable for reciprocating movement, it can also be fitted on rods and pistons.They are widely used in all applications from light duty to the heaviest working conditions.

Component: 1 piece energizing ring;1-8 pieces intermediate sealing rings;1 piece support ring.

Material:

Energizing ring: cotton fiber reinforced NBR or FKM;NBR or FKM; POM; Nylon; PTFE

Intermediate sealing ring: cotton fiber reinforced NBR or FKM;NBR or FKM;PTFE

Support ring: cotton fiber reinforced NBR or FKM;NBR or FKM; POM; Nylon, PTFE

Feature: High-pressure
resistance, high-temperature resistance.

Technical data:

Pressure:up to 40 MPa

Speed:up to 0.5 m/s

Temperature:up to 200 ℃ depending on rubber elastomer