설명
Having shorter outer sealing lip,U1 are desinged especially for piston applications.
기술 데이터:
Pressure: 400 bar
Temperature: -35 to +110℃
속도: 0.5m/s
매체: 유압 오일(광유 기반)
재질: PU
Hardness: 90-95 Shore A
Color: Blue
Advantages:
Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
간편한 설치