설명

V packing seals, also called vee cups, v packings, vee packing sets, vee packing seal, etc. They are composed of 3-10 lip rings made of cotton fiber reinforced rubber elastomer.
Boss Sealing Solutions vee packing seals are suitable for reciprocating movement, it can also be fitted on rods and pistons.They are widely used in all applications from light duty to the heaviest working conditions.
Component: 1 piece energizing ring;1-8 pieces intermediate sealing rings;1 piece support ring.
재질:
Energizing ring: cotton fiber reinforced NBR or FKM;NBR or FKM; POM; Nylon; PTFE
Intermediate sealing ring: cotton fiber reinforced NBR or FKM;NBR or FKM;PTFE
Support ring: cotton fiber reinforced NBR or FKM;NBR or FKM; POM; Nylon, PTFE
특징: High-pressure
resistance, high-temperature resistance.
기술 데이터:
Pressure:up to 40 MPa
Speed:up to 0.5 m/s
Temperature:up to 200 ℃ depending on rubber elastomer