Descrizione
R2 is a standard seal profile of hallite H605, it operates well in every hydraulic applications.
Technical Data
Pressure: below 400 Bar,
Temperature: -35 to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: High-grade PU
Hardness: 92 Shore A
Color:Turquoise
Advantages:
Insensibility against shock loads and pressure peaks
High resistance against extrusion
Perfect sealing performance under low pressure enven O-pressure
Easy installation