Product description: Compact Seal TPM,DBM

Descrizione

Hydraulic compact piston seal TPM

1. Applicazioni e proprietà

TPM also called DDAS/DAS/KDAS compact seal is a double acting seal and guide element, it is consist of 1 piece elastomer ring,2 pieces back up rings and 2 pieces guide rings.

Elastomer has an good sealing effect in both dynamic and static conditions,back up ring prevent the elastomer be extruded  into the sealing gap,the role of the guide ring is to help the piston in the cylinder guide and absorb the radial force.

it mainly used in hydraulic cylinders as a piston seal.

Application:

Bulldozers, excavators, loaders, cranes, hydraulic gate and agricultural machinery.

2. Materiali standard

Guide ring:POM

Back-up ring:PU

Elastomer:NBR

3. Condizioni di esercizio

Diameter Range: from 20mm to 250mm

Pressure Range:0-35 MPa

Temp Range: -30℃ to 120℃

Speed: <=0.5m/s

Fluido: olio idraulico, acqua, aria e fluidi scarsamente infiammabili.

4.Size

DN H9d1 h9L1 +0.2 +0.2d2 h9d3 h11L2 +0.1DBM Order No.TPM Order No.
201113.517192.1–TPM-20
221313.519212.1–TPM-22
25151221234–TPM-25
251512.52224498059TPM-25/1
251516.421.4523.56.3598059/1TPM-25/2
251613.522242.1–TPM-25/3
281913.525272.1–TPM-28
301715.426.528.56.35118066TPM-30
302113.527292.1–TPM-30/1
322215.528312.6–TPM-32/1
322216.428.530.56.35125086TPM-32
352515.531342.6–TPM-35/1
352516.431.433.56.35137098TPM-35
402418.435.438.56.35157094TPM-40
402615.536392.6–TPM-40/1
403012.536384157118TPM-40/2
403012.537394157118/1TPM-40/3
DN H9d1 h9L1 +0.2 +0.2d2 h9d3 h11L2 +0.1DBM Order No.TPM Order No.
403016.435.438.56.35157118/2TPM-40/4
422815.538412.6–TPM-42
452918.440.443.56.35177114TPM-45
453115.541442.6–TPM-45/1
453516.440.443.56.35177137TPM-45/2
503418.445.448.56.35196133TPM-50
503420.546493.1–TPM-50/1
553918.450.3653.56.35216153TPM-55
553920.551543.1–TPM-55/1
564020.552553.1–TPM-56
604418.455.458.56.35236173TPM-60
604420.556593.1–TPM-60/1
634718.458.461.56.35248185TPM-63
634719.458.461.56.35248185/1TPM-63/2
634720.559623.1–TPM-63/1
654920.561643.1–TPM-65/1
655018.460.463.56.35255196TPM-65
705022.464.268.36.35275196TPM-65/1
705420.566693.1–TPM-70
755522.469.273.36.35295216TPM-75
755920.571743.1–TPM-75/1
806022.474.1578.36.35314236TPM-80
806222.576793.6–TPM-80/1
856522.479.1583.36.35314255TPM-85
907022.484.1588.36.35354275TPM-90
907222.586893.6–TPM-90/1
957522.489.1593.36.35374295TPM-95
1007522.493.15986.35393275TPM-100
1008222.596993.6–TPM-100/1
1058022.498.11036.35413314TPM-105
1108522.4103.11086.3543334TPM-110
1109222.51061093.6–TPM-110/1
1159022.4108.11136.35452354TPM-115
1159722.51111143.6–TPM-115/1
1209522.4113.1118.16.35472374TPM-120
12510025.4118.11236.35492393TPM-125
12510326.51211245.1–TPM-125/1
13010525.4123.11286.35511413TPM-130/1
13010525.4122.6127.59.5511413/1TPM-130
13311522.4125.6130.59.52–TPM-133
13511025.4128.11336.35–TPM-135/1
13511025.4127.6132.59.5531433TPM-135
14011525.41331386.35551452/1TPM-140/1
14011525.4132.6137.59.5551452TPM-140
14011826.51361395.1–TPM-140/2
14512025.4138.3142.956.35–TPM-145/1
14512025.4137.6142.59.5570472TPM-145
DN H9d1 h9L1 +0.2 +0.2d2 h9d3 h11L2 +0.1DBM Order No.TPM Order No.
15012525.4142.6147.59.5590492TPM-150
15012525.41431486.35–TPM-150/1
15012826.51461495.1–TPM-150/2
152.412731.75145149.919.5–TPM-152.4
15513025.4147.6152.59.5610511TPM-155
15513025.41481536.35–TPM-155/1
16013025.4153157.56.35–TPM-160
16013025.4152.6157.59.5629531TPM-160/1
16013525.4152.6157.59.5–TPM-160/2
16013826.51561595.1–TPM-160/3
16514025.4157.6162.59.5649551TPM-165
17014525.4161.7167.112.7669570TPM-170
17014826.51661695.1–TPM-170/1
17515025.4166.7172.112.7688590TPM-175
18015035.4172.95177.876.35708590TPM-180
18015525.4171.7177.112.7708610TPM-180/1
18516025.4176.7182.112.7728629TPM-185
19016525.4181.718712.7748649TPM-190
19517025.4186.719212.7767669TPM-195
20017525.4191.619712.7787688TPM-200
20017531.51961996.6–TPM-200/1
21018525.4201.620712.7826728TPM-210
22019035.4212.7217.96.35866748TPM-220
22019525.4211.621712.7866767TPM-220/1
23020525.4221.622712.7905807TPM-230
24021525.4231.623712.7944846TPM-240
25022035.4242.9247.856.35984866TPM-250
25022525.4241.624712.7984886TPM-250/1