Tenuta in PTFE+15% vetro+5%MOS2

Greyish balck
Good wear resist
Self-lubracating
Product description: Good pressure resist and higer hardness

Descrizione

The filling of glass fiber and molybdenum disulfide enhances the compression, abrasion, and stretch resistance of PTFE, while maintaining good low friction and self-lubricating properties.

Please contact us for more details or other percentage filers.