PTFE rotary shaft seal is consists of a stainless steel skeleton and PTFE sealing lip. The common number of lips is single lip, double lip and three lips. Has good properties of low friction, high pressure resistance, low energy consumption and corrosion resistance, mainly be used as high pressure oil seals and air compressor oil seals.



Radial shaft seals featuring one or more PTFE sealing lips are designed to withstand aggressive environments, high temperatures, high pressures, and dry running—conditions that conventional radial shaft seals with elastomeric sealing lips cannot endure.
PTFE rotary shaft seal technical data:
Material: Stainless Steel+PTFE/Filled PTFE(Carbon/glass fiber/MOS2/Graphite)
Pressure: 20 MPa
Temperature: -60 ° C / +200 ° C
Speed: ≤40 m/s
lips: PTO(single lip), PTO2(double lips), PTO3(three lips), etc.
Dimensioni: su richiesta.