Chatta con noi, offerto da LiveChat

PTFE carbon gasket

Carbon filled PTFE
High-temperature resist
Good wear resist
Nero

Descrizione

This carbon fiber filled polytetrafluoroethylene PTFE makes the gasket has better wear resistance. Working temperature up to 260 ° C, widely used in high temperature conditions, such as high temperature air compressors, pumps, mixing tanks, centrifuges and so on.

The company produces all kinds of standard non-standard gaskets, pure polytetrafluoroethylene gaskets, various modified PTFE gaskets, carbon fiber filled PTFE gaskets, glass fiber filled PTFE gaskets, graphite filling PTFE gasket, molybdenum disulfide filled PTFE gasket, rubber gasket, PEEK gasket, POM gasket, nylon gasket, etc. Welcome to place an inquiry.

For more information or inquiry,please request.

sales@bosssealing.com

Skype: live:bosssealing

Richiedi un preventivo

Contattaci oggi stesso e ricevi una revisione aziendale e una consulenza gratuite.