Tubo in PU resistente all'idrolisi

Hydrolysis resistant
-40 d.c to +100 d.c
92 SHORE A
Red color
Product description: Good hydrolysis resistant properties,suitable for CNC manched seals.

Descrizione

Hydrolysis resistant casting polyurethane PU tube has excellent hydrolysis resistance properties, good stability in water and mineral oil at 90 degrees Celsius, suitable for metallurgy, steel, coal mining and other industries.

Dati tecnici:
Color: red
Hardness: 92 SHORE A
Density: 1.16g/cm3

Temperature: -40 degrees Celsius to 100 degrees Celsius

Please request if any need.