Product description: Piston Seal AQ

Descrizione

1. Applicazioni e proprietà

Suitable for high-speed, high-pressure. With low friction and high elasticity, good dynamic and static sealing performance, groove is simple, good sliding. Recommended for piston-type accumulators, indicating double-acting pistons such as cylinders and positioning cylinders.

2. Materiali standard

Slide Ring:filled PTFE

O-Ring:NBR/FKM.

X-Ring:NBR/FKM.

3.Size

Bore dia from 16 mm to 1000mm

Other general seal profile name:DAQ,JAQ