Petearje mei ús, mooglik makke troch LiveChat

Neopreen Kelvar K29 stof V-pakkingsring

Neoprene CR
Kelvar K29
aramid fabric reinforcement
packing seal

Beskriuwing

Neoprene CR Kelvar K29 faramid fabric reinforcement packing V ring

 

Material:Neoprene CR+ Kelvar K29

Hardness: 60 shore A ±10%

Operating temperature: -10℃-+150℃

 

Foardiel:

1.permanent heat and flame retardant.

2. permanent resistance to acid and alkali and organic solvents.
3. high strength, high wear resistance, high tear resistance.
4. No droplets are produced in case of fire, and no toxic gas is produced.

 

Kelvar is a trade mark of Dupont

Freegje in offerte oan

Nim hjoed kontakt mei ús op en krije in fergees bedriuwsresinsje en konsultaasje.