BD heavy duty rod seals include 1 piece PU seal,1 piece NBR O-Ring and 1 piece POM back-up ring,it provide a safe sealing property with their double dynamic sealing lips and POM back up ring. The NBR ring in this design provides maximum sealing even in low pressures.
Technical Data
Pressure: 500 Bar
Temperature: -35 to +110 ℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material
Material: PU+POM+NBR
Color: Blue, Dark green
Advantages
High resistance to high temperature
High abrasion resistance
Low compression set
Easy installation